Abbott's American Watchmaker and Jeweler

How to true a balance, repair a chipped dial, temper a spring or test a stone — the working bench-book of the American watch trade, arranged A to Z.

HomeT › To Frost Silver (Produce a frosted surface upon)

To Frost Silver (Produce a frosted surface upon)

To produce a frosted surface upon polished silver use cyanide of potassium with a brush; the silver should not be handled during the process, but held between pieces of boxwood or lancewood. The proportion should be, 1 ounce of cyanide of potassium in 1 pint of water.

← To Clean Silver PlateTo Frost Silver (Goods may be frosted) →