Home › Cements And Uniting Bodies › Orange Enamels
Orange Enamels
I. Red lead, VI. Tin, 2 to 5 parts; lead, 10 parts; cal- 12 parts; red sulphate of iron and oxide of cine in an iron pot at a dull cherry-red heat, antimony, of each 1 part; flint powder, 3 and scrape off the oxide as it forms, observing parts; calcine, powder, and melt with flux, 50 to obtain it quite free from undecomposed parts. metal; when enough of the dross is obtained, II. Red lead, 12 parts; oxide of antimony, reduce it to fine powder by grinding and elu- 4 parts; flint powder, 3 parts; red sulphate of triation (see No. 14), then mix 4 parts of this powder with an equal weight of pure sand or powdered flints, and 1 of sea-salt, or other alkaline matter; fuse the mixture in a Hessian crucible, and proceed as before. The best proportions of the tin and lead, for all ordinary purposes, are about 3 of the former to 10 of the latter. The calcined mixed oxides are commonly called calcine.
VII. Lead and tin, equal parts; calcine as above; and take of the mixed oxides, or calcine (see preceding receipt) and ground flints, of each 1 part; pure subcarbonate of potash, 2 parts; as before.
VIII. Lead, 30 parts; tin, 33 parts; calcine as before, then mix 50 parts of the calcine with an equal weight of flints, in powder, and 1 pound of salts of tartar; as before. A fine dead white enamel.