Work the goods for 20 minutes in a bath containing 1 ounce peachwood or limawood, 2 ounces logwood and 1/2 ounce fustic; lift, and add 1 ounce copperas in solution; stir well and work in this for 30 minutes; lift out and expose to the air for a short time; wash and dry. Different the general rule that woolens must be worked at a boiling heat.
To dye 5 pounds of woolen goods-work for 20 minutes in a bath with 1 pound ferrocyanide of potassium, and lift; then take 1/2 pint nitrate of iron and add to it 1 ounce crystals of tin (or 1 pint chloride of tin); stir well for a few minutes and then add this mixthis mixture to the bath, and work the goods in this for 30 minutes; wash out and dry. For various shades of color, increase or diminish the quantities in proportion.