Etching Fluid for Copper
Aquafortis, 2 ounces; water, 5 ounces. Mix. 2962. Callot's Eau Forte for Fine Touches. Dissolve 4 parts each of verdigris, alum, sea salt, and sal ammoniac, in 8 parts vinegar; add 16 parts water, boil for a minute, and let it cool.